ASTM F1306 Puncture Fixture Setup and Operation

Home / Testing Guides / ASTM F1306 Puncture Fixture Setup and Operation

This post will help guide you through ASTM F1306 Puncture Fixture setup and operation on your universal testing machine. More information on performing ASTM F1306 can be found here.

More information on our puncture fixture offerings can be found here.

Puncture fixture diagram for ASTM F1306 testing

Installation

  1. Slide the fixture base onto the male eye end on the fixed crosshead.
  2. Align male and female eye end pin holes and insert the pin from the front of the machine.
  3. Tighten jam nut against the fixture base to eliminate axial play between the fixture and the eye end.
  4. Slide probe onto the male eye end on the moving crosshead.
  5. Align the male and female eye end pin holes and insert the pin from the front of the machine.
  6. Tighten jam nut against probe to eliminate axial play between the probe and the eye end.

Grip Use

  1. Cut the sample material to size (3”x 3” square min.)
  2. Place sample in fixture.
  3. Place the clamping ring over the sample. Be sure to align the alignment arrows on the clamping ring and the fixture base.
  4. Secure the clamping ring by rotating clockwise until the sample is firmly held in place.
    • For systems with less than 5” deep testing spaces, it is recommended that the handles be removed from the clamping ring to allow full rotation.
  5. Inspect the test material for proper tension. The exposed portion of the sample should be flat, not indented or bubbled.

Maintenance

  1. Clean fixture after use. Wipe away sample fragments or residue.
  2. This fixture does not require lubricant.
  3. If fixture becomes worn or damaged, contact ADMET for a replacement.
ASTM F1306 puncture fixture

By: Kevin Weiler | Published on: September 27, 2016 | Last Updated: January 6, 2026

Just Ask!

Have a question about ADMET puncture fixtures?

We’re ready to help!

spiral arrow graphic

Testing Guides

  • Medical Adhesive Testing Basics

    Medical adhesives are specialized substances used to bond medical devices, tissues, or other components together. They must comply with strict biocompatibility requirements and are vital in surgeries, wound care, and medical equipment manufacturing.
  • Deflection & How To Use A Deflectometer

    Deflection, in materials science, is the amount a material deflects under compressive load. It is a displacement measurement with units expressed in millimeters or inches. This post goes over frequently asked questions around deflection measurements and equipment used to measure them.
  • Peel Strength Testing

    Peel strength is calculated by averaging the load to peel the specimen and dividing it by unit width of the bond line.
  • Tensile Testing FAQs

    Tensile testing FAQs including How does the loading rate affect tensile properties? How does grip-specimen engagement affect tensile properties? What is the best way to measure small strains? are answered.