In this post, we will show you how to set up MTESTQuattro to set specimen geometry for o-ring specimens. O-ring testing can be accomplished with an eXpert 7600 single column testing system and a set of specialized o-ring tensile fixtures.
With MTESTQuattro running, navigate to the specimen tab.
Selecting Geometry
- For Flat O-Rings:
- In MTESTQuattro, go to the Specimen tab of the active test procedure.
- Select Flat O-Ring as geometry type (Figure 1).

Figure 1 – Selecting Flat O-Ring Geometry
- For Round O-Rings:
- In MTESTQuattro, go to the Specimen tab of the active test procedure.
- Select Round O-Ring as geometry type (Figure 1).

Figure 2 – Selecting Round O-Ring Geometry
Selecting Analysis
- In MTESTQuattro, go to the Analysis tab of the active test procedure.
- Select User as the analysis suite.
- Highlight O-Ring and click Select.
- O-Ring should now be listed in the selected analysis section.

Figure 3 – O-Ring Analysis Enabled
Running a Test
- Measure specimen
- Update specimen dimensions in MTESTQuattro if necessary (Figure 4).
- Perform test.
- After the test has completed, the Tensile Strength (psi) and Elongation (%) will be calculated.

Figure 4 – Updating Specimen Geometry