Please see below for a list of grips and fixtures that are not standard but are essential to test certain products. We also design custom-built fixtures for samples that cannot be clamped by listed fixtures. Contact ADMET for more information.

The o-ring test fixture is a motorized test fixture to test rubber o-rings per ASTM D1414. The GSP-ORT fixture is supplied with steel rollers.
— Force Capacity: 10kN
— Rotation Speed: Up to 17 rpm (non-motorized configuration is also available)
— Roller Diameter Options (mm): 3.18, 4.5, 4.75, 6.35, 12.7, 15, 18.3, 20, 22.3, 25, 28.3

ADMET FS-CFT is used to determine the static and kinetic coefficients of friction of plastic film and paper. A single sheet of the test specimen is clamped securely to a horizontal bed and another sheet of specimen is clamped to under the FS-CFT sled. As the sled moves, the force required to overcome the frictional resistance between two surfaces is measured and recorded.
— Force Capacity: 500N
— Available Platen Options: 270 x 150mm, 470 x 150mm, 570 x 150 mm
— Sled Surface Options: Cellular rubber (ASTM D1894), Felt (ISO 8295)

— Force Capacity: Up to 12kN
— Hook Diameter: Up to 16mm
— Made-to-order configurations also available.

— Force Capacity: Up to 20kN
— Roller Diameter: up to 101.6mm
— Made-to-order configurations also available.

— Force Capacity: Up to 400kN
— Coupling: Eye ends, threaded ends (SI and metric)
— Made-to-order configurations also available