These grips are applicable for webbings and ribbons. The webbing is fed through the center slot, the drum is rotated and then pinned to lock it in place. As the material is pulled it tightens on itself keeping it from slipping. The drums offer stress relief to prevent the breakage of the specimen in the clamping area.
GRW-100T

- Tensile Force: 100kN
- 60 mm Ø roll, 80mm wide
- 60 mm Ø roll, 100mm wide
- 60 mm Ø roll, 120mm wide
- 80 mm Ø roll, 120mm wide
- Download GRW-100T Datasheet
GRW-200T

- Tensile Force: 200kN
- 100 mm Ø roll, 200mm wide