90 Degree Adhesive Peel Strength Test on a Universal Testing Machine

This video shows a 90 degree adhesive peel strength test on an ADMET eXpert 7601 universal testing machine (tensile testing machine).  We fit the eXpert 7601 with our 90 degree peel strength fixture and one vise grip on the top crosshead to h...

By |April 12th, 2010|Products, Video|Comments Off on 90 Degree Adhesive Peel Strength Test on a Universal Testing Machine

ASTM F2458 – Wound Closure Strength of Tissue Adhesives

Materials that adhere living tissues together are being used more frequently in surgical procedures as adjuncts to sutures or as replacements. ASTM F2458 - 05 is a standard test method for determining the comparative wound closure strength of tissue a...

By |March 1st, 2010|Test How To's|Comments Off on ASTM F2458 – Wound Closure Strength of Tissue Adhesives