Biomaterials

Home/Tag:Biomaterials

Dental Adhesive, Composite Resin, and Ceramic Material Tensile, Shear, and Flexural Testing System

Dental materials ranging from composite resin fillings, to porcelain to metal crowns and bridges, to alginate impression material, to dental adhesives for bonding and restorative dentistry are all tested for their mechanical property strengths. ISO 687...

By |June 1st, 2011|Testing Issues|Comments Off on Dental Adhesive, Composite Resin, and Ceramic Material Tensile, Shear, and Flexural Testing System

ASTM F2258- Tensile Strength Tissue Adhesive -Wound Closure Testing System

ASTM F2258 describes the testing procedure to obtain data to compare adhesive strengths of tissue adhesives intended for use as surgical adhesives or sealants, or both on soft tissue.  Preparing the Test Substrate is a critical part of this specif...

By |September 14th, 2010|Test How To's|Comments Off on ASTM F2258- Tensile Strength Tissue Adhesive -Wound Closure Testing System

Testing System for Bioabsorbable Plates and Screws – ASTM F2502

ASTM F2502 is a standard for testing Bioabsorbable Plates and Screws for Internal Fixation Implants. These types of plates and screws are resorbed into the body once implanted to unstable bone or tissue connected to bone. The advantage over a metallic ...

By |August 11th, 2010|Test How To's|Comments Off on Testing System for Bioabsorbable Plates and Screws – ASTM F2502

ASTM F2458 – Wound Closure Strength of Tissue Adhesives

Materials that adhere living tissues together are being used more frequently in surgical procedures as adjuncts to sutures or as replacements. ASTM F2458 - 05 is a standard test method for determining the comparative wound closure strength of tissue a...

By |March 1st, 2010|Test How To's|Comments Off on ASTM F2458 – Wound Closure Strength of Tissue Adhesives

UNCC receives ADMET Torsion Tester for Bioactive Bone Screws

The Orthopedic Tissue Engineering and Materials Lab at the University of North Carolina Charlotte (UNCC) was the winner of ADMET, Inc's 20 year anniversary celebration biomedical testing system giveaway. Drs. Ahmed El-Ghannam and Nigel Zheng at UNCC he...

By |February 2nd, 2010|News|Comments Off on UNCC receives ADMET Torsion Tester for Bioactive Bone Screws