Automatic Concrete Cylinder Tester for ASTM C39 Strength Reports

All concrete testing laboratories produce essentially the same compressive strength test reports. So, how can a laboratory manager create a distinctive product while boosting profitability? Speed ControlConcrete exhibits loading-rate sensitivity relati...

By |April 20th, 2010|Products|Comments Off on Automatic Concrete Cylinder Tester for ASTM C39 Strength Reports

Rubber Seal Compression Testing to Obtain Load vs. Deflection Curve

This video shows a compression test on a rubber door seal to obtain the load vs. deflection curve and to determine the load at various displacements.  For example, our customer wanted to know the load at 5, 15, and 30% compression of the original ...

By |March 26th, 2010|Video|Comments Off on Rubber Seal Compression Testing to Obtain Load vs. Deflection Curve