ASTM E606 describes the determination of fatigue properties of nominally homogeneous materials via strain-controlled cyclic loading. Strain-controlled fatigue testing is a unique test method as cyclic stresses and strains can be determined at any time during this test. Note that differences in strain histories other than constant-amplitude alter fatigue life compared with the constant amplitude results.
Before conducting ASTM E606, it is important to read the entire specification in the relevant ASTM publication.
ASTM E606 | Metals | Fatigue Testing
- Prepare the test specimens. Measure and record the thickness and the width of the reduced section of each specimen.
- Place the specimen in the tensile grips ensuring proper alignment and attach the extensometer.
- Apply the load at least until failure.
- Record total accumulated cycles to failure (and fracture).
Calculations:
- Relaxed stress or of creep strain
- Total relaxation or keep
- Change in the amount of inelastic strain during hold
- Total number of cycles to failure
- Cyclic strain hardening exponent
- Cyclic strength coefficient
- Fatigue strength exponent
- Fatigue ductility exponent
- Fatigue strength coefficient
- Fatigue ductility coefficient
ASTM E606 | Metals | Fatigue Testing
- Tensile specimen pulled to fracture. Depicts region where necking occurred
ASTM E606 | Metals | Fatigue Testing
ASTM E606 | Recommended Equipment |
---|---|
Testing System | |
Fixturing | |
Accessories |
Ask our Engineers
Just have a quick question about running ASTM E606 on your system?
We're happy to help!
Ask our Engineers