A Simplification of IFD Foam Testing

Home / Testing Guides / A Simplification of IFD Foam Testing

Foam is both a versatile and crucial substance found in a wide variety of products including safety equipment, foam cushions in furniture, insulation & thermal protection, automobile interiors & sound deadening, carpet padding & flooring installations, shipping & packaging, shoes & apparel, mattresses & bedding, marine applications, and much more. It is hard to imagine our modern world without foam and foam products.

Image of compression platen for ASTM D3574 B1 force deflection test on foam

Materials testing systems are one option to consider when managing quality control of foam products. Foam testing is often concentrated on Indentation Force Deflection (IFD), a method for determining the firmness, stiffness, and load bearing capacity of the materials.

IFD measures the load required to depress a 50 square inch compression platen into a polyurethane foam specimen. These mechanical properties are influenced by the thickness and size of the sample. In essence, IFD measures firmness, which could be an essential part of chairs, couches and other furniture.

Before the existence of polyurethane foam, rubber latex foams were in wider use and the standard for measuring firmness was called RMA (Rubber Manufacturer’s Association), according to a publication from the Polyurethane Foam Association. RMA was executed in a similar way to IFD measurements of today.

While IFD plays a role in the comfort of a seat cushion, it is not the only factor, as tensile, tear, elongation, and recovery time tests are all part of the equation. This is represented as the number of pounds at a deflection percentage of the height of the specimen (ex. 40 lbs/50 square inches at a 30 percent deflection on a four inch thick sample).

Accuracy is a very important factor when measuring the Indentation Force Deflection. Manufacturers of foam and foam products come to ADMET in order to test their foam products because of our accurate and customizable systems as well as cost-effective results.

The eXpert 5600F foam testing system can perform IFD tests as well as tensile, compression, elongation, recovery time, and tear measurements. For those who need to determine the fatigue capabilities of their materials, the eXpert 5900F fatigue foam testing system can perform the same tests as the 5600F testing machine and can also conduct fatigue tests. These machines as well as ADMET’s software exceed international testing standards and can determine ASTM D3574 and ISO 2439 among other foam testing specifications.

All types of foam can be tested on these particular ADMET machines including open-cell, closed-cell, latex, polyurethane, and reticulated. The eXpert 5600F series along with machine controllers and tension compression actuators fit a frame created specifically for testing foam specimens.

Some of the features of this machine include wide tensile grips for holding thicker foam samples, a circular indenter and swivel joint, the ability to quickly transfer between tensile and compression tests, and pre-installed foam test methods and analysis on the MTESTQuattro PC-based controller.

During an IFD test, the MTESTQuattro software charts live load and foam height over time. A report from the controller consists of the force of deflection, support factor, specimen identifier, load, and time. This controller offers flexibility with regard to control, data obtainment, analysis, and reporting.

ADMET staff developed the eXpert 5600F Series after working with leading companies within the foam industry and determining that typical universal testing machines do not adequately meet the needs of most foam manufacturers. These systems did not provide enough horizontal space for testing larger samples, were too large, and were prohibitively expensive.

The eXpert 5600F Series solved these problems through a design that was specific to foam specimens. This shows how the ADMET engineering team is capable of customizing and developing testing systems according to the specifications of its customers. ADMET materials testing machines are supported for life, exceed all ASTM and ISO testing requirements, and are easy to install and use. To learn more about our foam testing machines, please contact us below.

By: Kevin Weiler | Published on: March 18, 2013 | Last Updated: January 6, 2026

Just Ask!

Have a question about foam testing?

We’re ready to help!

spiral arrow graphic

Testing Guides

  • Medical Adhesive Testing Basics

    Medical adhesives are specialized substances used to bond medical devices, tissues, or other components together. They must comply with strict biocompatibility requirements and are vital in surgeries, wound care, and medical equipment manufacturing.
  • Deflection & How To Use A Deflectometer

    Deflection, in materials science, is the amount a material deflects under compressive load. It is a displacement measurement with units expressed in millimeters or inches. This post goes over frequently asked questions around deflection measurements and equipment used to measure them.
  • Peel Strength Testing

    Peel strength is calculated by averaging the load to peel the specimen and dividing it by unit width of the bond line.
  • Tensile Testing FAQs

    Tensile testing FAQs including How does the loading rate affect tensile properties? How does grip-specimen engagement affect tensile properties? What is the best way to measure small strains? are answered.