How to Perform ASTM D1037 Wood-Base Fiber and Particle Panel Strength Testing

Home / Testing Standards / ASTM D1037 Wood-Base Fiber and Particle Panel Strength Testing

Summary of Test

ASTM D1037 contains a number of test methods and specifications designed to identify the properties of wood-base fiber and particle panel materials. The properties range from size and appearance, to tensile, compression, and shear strengths, as well as hardness, water absorption, and fastener holding. The information included on this page will focus on the mechanical tests within ASTM D1037 that are the most common and best performed on a universal testing machine to identify typical mechanical properties.

Before conducting ASTM D1037, it is important to read the entire specification in the relevant ASTM publication.

Recommended Equipment

Testing Procedure

Static Bending

  1. Prepare the specimens as described in the test method – using specimens cut from both directions with respect to original board, in dry and soaked conditions.
  2. Mount the specimen in a 3-point (center loading) fixture. Selection of the proper fixture span, supports, and loading nose will depend on specimen size and condition.
  3. Apply load to the center of the specimen at the constant rate of speed calculated from the equation in the standard.
  4. Continue the test until rupture, while recording all force vs. deflection data.

Calculations:

  • Modulus of Rupture
  • Stiffness (Apparent Modulus of Elasticity)

Tensile Strength Parallel to Surface (dog-bone specimens)

  1. Prepare the specimens as described in the test method – using dog-bone shapes cut from both directions with respect to original board, in dry and soaked conditions.
  2. Mount the specimens in self-aligning and self-tightening grips.
  3. Apply a tensile load at the constant rate of speed specified in the standard.
  4. Continue loading until failure.

Calculations:

  • Max Load
  • Max Stress

Tensile Strength Perpendicular to Surface (block-type specimens)

  1. Prepare the specimens as described in the test method – dry condition only.
  2. Bond the test specimen to test blocks on both sides and mount the assembly into the appropriate loading fixtures.
  3. Apply a tensile load at the constant rate of speed specified in the standard.
  4. Continue loading until failure.

Calculations:

  • Max Load
  • Max Stress

Compression Strength Parallel to Surface

  1. Determine the Procedure within this method that best matches your test material characteristics: Procedure A (Laminated Specimen), Procedure B (Lateral Support), or Procedure C (Short Column).
  2. Prepare the specimens as described in the test method and selected procedure – both in the dry and soaked conditions.
  3. Load the specimens into the test machine, centered underneath a spherically seated compression platen.
  4. Apply a compressive load at the constant rate of speed specified in the standard.
  5. Continue loading until failure.

Calculations:

  • Max Stress (Crushing Strength)
  • Modulus of Elasticity

Other test procedures within ASTM D1037 that could be performed using a universal testing machine include:

  1. Lateral Nail Resistance
  2. Nail Withdrawal
  3. Nail Pull-Through
  4. Direct Screw Withdrawal