Summary of Test
Specification ASTM D751 includes test methods for covering a wide range of mechanical properties of coated fabrics. A coated fabric is a material that has at least one layer of a textile and one layer of a polymeric substance. Examples would be tarps, outdoor clothing, and rain wear. Some of these tests require specialized equipment (hydrostatic resistance, blocking, wicking, impact, etc.), but most of these tests can be performed using a Universal Testing Machine.
Recommended Equipment
ASTM D751 Testing System Requirements
- Straining mechanism
- Clamps for holding specimens
- Load and elongation recording mechanisms.
ADMET universal testing machines include the straining mechanism (item 1) and built-in load and elongation recording mechanisms (Item 3). The clamps (Item #2) are devices that get pinned to the universal testing machine and are designed specifically to hold each of the materials/samples described in each of the various tests listed above.
Required Equipment for Each Type of ASTM D751 Test
- Breaking Strength — Procedure A: Grab Test Method
- Vise Grips (Top grip mounted on universal joint)
- Front Jaw Inserts: 25mm tall x 25mm wide
- Rear Jaw Inserts: 25mm tall x 50mm wide
- Vise Grips (Top grip mounted on universal joint)
- Breaking Strength — Procedure B: Cut Strip Test Method
- Same grips as Procedure A.
- Elongation
- Test is done at the same time as the breaking strength test so grips are the same.
- Bursting Strength
- This fixture holds a piece of fabric securely on the top and bottom surface an exposed a circular area of fabric. The other part of the fixture is a polished steel ball that is mounted to the top of the machine which is used to burst the fabric.
- Puncture Resistance
- This fixture is the same as used for the bursting test but the polished steel ball is replaced with a sharp pointed instrument.
- Tearing Strength — Procedure B: Tongue Tear Method
- Same vise grips used for the Breaking Strength test but replaced the 25mm x 25mm front jaws with 25mm tall x 50mm wide jaws so you have a set of four 25mm x 50mm jaws.
- Trapezoidal Tear
- Same vise grips used for the Tearing Strength test
- Adhesion Coating to Fabrics
- Same vise grips but jaws should be 25mm tall x 75mm wide
- Tack-Tear Resistance
- This test requires a specialized grip fixture that is used only for this test. It is complicated, and the design can be seen in the specification.
- Seam Strength
- Same grips as described in Adhesion Coating to Fabrics test
- Dead Load Seam Strength
- Same vise grips as specified in the other tests
- Crush Resistance
- This test deflects the material over a button-shaped compression platen until the material is crushed or cut. This test requires a unique compression fixture, the exact dimensions of which can be found in the specification.
Just Ask!
Questions about running ASTM D751 on your system?