EX-3542 Clip-on Axial Extensometer

— Available Gauge Lengths: 10mm, 12.5mm, 25mm, 35.6mm, 50mm, 0.5″, 0.64″, 1.0″, 1.4″, 2″
— Extension: +/- 5, 10 , 20, 25%, +50%/- 10%, and +100%/-5%
— Excitation: 5 to 10 VDC recommended, 12 VDC or VAC max
— Output: 2 to 4 mV/V, nominal, depending on model
— Linearity: 0.10% to 0.15% of full scale measuring range, depending on model
— Meets existing ASTM class B-1 and ISO 9513, class 0,5 requirements for accuracy