EX-3543 Long Travel Clip-on Axial Extensometer
— Gauge Length: 100mm (4″)
— Travel: 500mm (2″) or 100mm (4″)
— Excitation: 5 to 10 VDC recommended, 12 VDC or VAC max Output: 2 to 4 mV/V nominal, depending on model
— Linearity: 0.15% of full scale measuring range
— Includes quick attach kit and various knife edges for flat and round specimens
— May be left on through specimen failure. The unit is designed so that the two halves of the extensometer come apart to prevent damage at specimen failure
— Full bridge, 350 ohm strain gauged design for compatibility with nearly any test system
— All standard units meet existing ASTM class B-1 and ISO 9513, class 0,5 requirements for accuracy
— Hardened tool steel knife edges are easily replaced. A spare set comes with every extensometer