A valued customer was interested in adding to their R&D lab’s testing capabilities to perform adhesion/cohesion tests on their thermal spray coatings per ASTM C633. This test involves loading the coating bond up to 100 kN (22,500 lbf) and is typically performed on a floor standing testing system to accommodate that high a force range. However, ADMET configured our cost-effective, unique-in-the-industry eXpert 2614 100 kN Table Top Universal Testing System for this application.

The eXpert 2614 can accommodate forces up to 100 kN, serving as a more cost-effective option than a floor standing unit. The customer can now perform high force tests on their thermal spray coatings, and can add capability in the future for a wide range of tensile, compression, and flexural tests on their materials.
ADMET also provided the customer with a sample preparation fixture to be able to bond up to 10 test pieces at one time, drastically increasing the efficiency and throughput of the testing.


Contact us today to learn more about how ADMET can configure Universal Testing Systems to maximize the efficiency of your in-house testing and support your testing requirements. We work closely with our customers to provide the most economical solution by configuring directly to their specific needs, without sacrificing capability, control, or performance.
By: Deniz Yalcin | Published on: August 1, 2024 | Last Updated: March 12, 2026
Just Ask!
Our systems are designed to meet your requirements.
Whether you need a standard solution or something more customized, our engineers can help!